Sometimes it is found that after a few days of injection molding, white and other light-colored PVC parts will find many small pits on the surface and have to be scrapped. The reason is related to the order of injection molding production.

When producing dark parts such as black or blue, due to hot air baking ingredients, many colors and dust will float in the air around the oven. If white PVC plastic parts are produced within the range where the dust is flying, the colored dust will fall on the white PVC parts, but the dust cannot be seen with the naked eye.

After a few days, the toner diffused and the range of pollution gradually increased, and it slowly turned into blue or black pits that could be seen clearly, and the injection molded parts had to be beaten.

Therefore, when producing light-colored PVC parts such as white, there must not be dark parts such as black or blue in production nearby.

To learn more about our manufacturing capabilities and discover what makes us different, please visit our website. If you’re ready to jump into your next project with us. No matter your need, contact us now and we not only meet your requirements, but we actively look for ways to improve on your product and thus save you money and time in today’s competitive marketplace.

Injection Molding, Plastic Mold Case, Plastic Molding Design, Plastic Parts
About admin

Leave a Reply

Your email address will not be published. Required fields are marked *

Need Help? Chat with us

Click one of our representatives below

  • Edward

    Manager

Need Help? Chat with us

Click one of our representatives below

  • Edward

    Manager

Need Help? Chat with us

Click one of our representatives below

  • Edward

    Manager